AISI 1018 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
AISI 1018 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round Categories: Metal
AISI 1018 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round Categories: Metal
AISI 1018 Steel, cold drawn, high temperature, stress relieved, 22-32 mm (0.875-1.25 in) round Categories: Metal
AISI 1018 Steel, cold drawn, high temperature, stress relieved, 32-50 mm (1.25-2 in) round Categories: Metal
AISI 1018 Steel, cold drawn, high temperature, stress relieved, 50-76 mm round Categories: Metal
AISI 1018 Steel, carburized at 925°C (1700°F), box cooled, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper. 19-32 mm (0.75-1.25 in) round Categories: Metal
Overview of materials for Cast Iron Categories: Metal
Overview of materials for Chrome-moly Steel Categories: Metal
Overview of materials for Ductile Iron Categories: Metal
Overview of materials for Duplex Categories: Metal
Overview of materials for Malleable Iron Categories: Metal