标准: | DIN 17456, DIN 17458, DIN 17459 , EN10216-5 TC 1 & 2 , EN10204-3.1 , NACE 0175 | 材料 | 1.4301, 1.4307 ,1.4401 ,1.4404, 1.4571 ,1.4438 |
---|---|---|---|
无损检测: | ET, UT, HT | 包装 | 胶合木箱/铁箱/带塑料盖的捆绑箱 |
强光 | 热回收管, 无缝不锈钢管 |
Stainless Steel Heat Exchanger Tube ASTM A213 TP304 304L TP317 TP321 With High Performance,Pickled Annealed ,Plain End
等级 | 材料 编号 | C | Si | 锰 | P | S | N | Cr | 莫 | 倪 | Ti | 其他人 |
铁素体或马氏体钢 | ||||||||||||
X2CrTi12 | 1.4512 | 0.030 | 1.00 | 1.00 | 0.040 | 0.015 | 10.50 至 12.50 | 6×(C+N)to0.65 | ||||
X6CrAl13 | 1.4002 | 0.08 | 1.00 | 1.00 | 0.040 | 0.015 | 12.00 至 14.00 | 0.10 至 0.30Al | ||||
X6Cr17 | 1.4016 | 0.08 | 1.00 | 1.00 | 0.040 | 0.015 | 16.00 至 18.00 | |||||
X3CrTi17 | 1.4510 | 0.05 | 1.00 | 1.00 | 0.040 | 0.015 | 16.00 至 18.00 | 4×(C+N)+0.15 至 0.80 | ||||
X12Cr13 | 1.4006 | 0.08 至 0.15 | 1.00 | 1.50 | 0.040 | 0.015 | 11.50 至 13.50 | 0.75 | ||||
奥氏体钢 | ||||||||||||
X5CrNi18-10 | 1.4301 | 0.07 | 1.00 | 2.00 | 0.045 | 0.015 | 0.11 | 17.00 至 19.50 | 8.00 至 10.50 | |||
X2CrNi19-11 | 1.4306 | 0.030 | 1.00 | 2.00 | 0.045 | 0.015 | 0.11 | 18.00 至 20.00 | 10.00 至 12.00 | |||
X2CrNiN18-10 | 1.4311 | 0.030 | 1.00 | 2.00 | 0.045 | 0.015 | 0.12 至 0.22 | 17.00 至 19.50 | 8.50 至 11.50 | |||
X6CrNiTi18-10 | 1.4541 | 0.08 | 1.00 | 2.00 | 0.045 | 0.015 | 17.00 至 19.00 | 9.00 至 12.00 | 5×C 至 0.70 | |||
X6CrNiNb18-10 | 1.4550 | 0.08 | 1.00 | 2.00 | 0.045 | 0.015 | 17.00 至 19.00 | 9.00 至 12.00 | 10×Cto1.00Nb | |||
X5CrNiMo17-12-2 | 1.4401 | 0.07 | 1.00 | 2.00 | 0.045 | 0.015 | 0.11 | 16.50 至 18.50 | 2.00 至 2.50 | 10.00 至 13.00 | ||
X2CrNiMo17-12-2 | 1.4404 | 0.030 | 1.00 | 2.00 | 0.045 | 0.015 | 0.11 | 16.50 至 18.50 | 2.00 至 2.50 | 10.00 至 13.00 | ||
X6CrNiMoTi17-12-2 | 1.4571 | 0.08 | 1.00 | 2.00 | 0.045 | 0.015 | 16.50 至 18.50 | 2.00 至 2.50 | 10.50 至 13.50 | 5×C 至 0.70 | ||
X2CrNiMoN17-13-3 | 1.4429 | 0.030 | 1.00 | 2.00 | 0.045 | 0.015 | 0.12 至 0.22 | 16.50 至 18.50 | 2.50 至 3.00 | 11.00 至 14.00 | ||
X2CrNiMo18-14-3 | 1.4435 | 0.030 | 1.00 | 2.00 | 0.045 | 0.015 | 0.11 | 17.00 至 19.00 | 2.50 至 3.00 | 12.50 至 15.00 | ||
X3CrNiMo17-13-3 | 1.4436 | 0.05 | 1.00 | 2.00 | 0.045 | 0.015 | 0.11 | 16.50 至 18.50 | 2.50 至 3.00 | 10.50 至 13.00 | ||
X2CrNiMoN17-13-5 | 1.4439 | 0.030 | 1.00 | 2.00 | 0.045 | 0.015 | 0.12 至 0.22 | 16.50 至 18.50 | 4.00 至 5.00 | 12.50 至 14.50 |
热交换器、冷凝器和锅炉用管尺寸 | |||||||||
外径 | BWG | ||||||||
25 | 22 | 20 | 18 | 16 | 14 | 12 | 10 | ||
壁厚 毫米 | |||||||||
0.508 | 0.71 | 0.89 | 1.24 | 1.65 | 2.11 | 2.77 | 3.40 | ||
毫米 | 寸 | 体重 公斤/米 | |||||||
6.35 | 1/4 | 0.081 | 0.109 | 0.133 | 0.174 | 0.212 | |||
9.53 | 3/8 | 0.126 | 0.157 | 0.193 | 0.257 | 0.356 | 0.429 | ||
12.7 | 1/2 | 0.214 | 0.263 | 0.356 | 0.457 | 0.612 | 0.754 | ||
15.88 | 5/8 | 0.271 | 0.334 | 0.455 | 0.588 | 0.796 | 0.995 | ||
19.05 | 3/4 | 0.327 | 0.405 | 0.553 | 0.729 | 0.895 | 1.236 | ||
25.4 | 1 | 0.44 | 0.546 | 0.75 | 0.981 | 1.234 | 1.574 | 2.05 | |
31.75 | 1 1/4 | 0.554 | 0.688 | 0.947 | 1.244 | 1.574 | 2.014 | 2.641 | |
38.1 | 1 1/2 | 0.667 | 0.832 | 1.144 | 1.514 | 1.904 | 2.454 | 3.233 | |
44.5 | 1 3/4 | 1.342 | 1.774 | 2.244 | 2.894 | 3.5 | |||
50.8 | 2 | 1.549 | 2.034 | 2.574 | 3.334 | 4.03 | |||
63.5 | 2 1/2 | 1.949 | 2.554 | 3.244 | 4.214 | 5.13 | |||
76.2 | 3 | 2.345 | 3.084 | 3.914 | 5.094 | 6.19 | |||
88.9 | 3 1/2 | 2.729 | 3.609 | 4.584 | 5.974 | 7.27 | |||
101.6 | 4 | 4.134 | 5.254 | 6.854 | 8.35 | ||||
114.3 | 4 1/2 | 4.654 | 5.924 | 7.734 | 9.43 | ||||
管材形式直管、U 形弯管、翅片管和盘管 | |||||||||
不锈钢管:A/SA213, A/SA249, A/SA268, A/SA269, A/SA789, EN10216-5, A/SA688, B/SB163, JIS-G3463, GOST9941-81。 | |||||||||
碳钢和合金钢管:A/SA178, A/SA179, A/SA192, A/SA209, A/SA210, A/SA213 |
S要求:
ASME SA213/A213:无缝铁素体和奥氏体合金--标准规范
钢制锅炉、过热器和不锈钢换热管。
ASTM A249 / A249M:焊接奥氏体钢锅炉、过热器标准规范
热交换器和冷凝管。
其他标准:DIN 17456 , DIN 17458, EN10216-5, JIS-G3463,...
材料等级:
尺寸 范围:
生产 | 外径 | 壁厚 |
换热管 | 6.00 毫米至 101.6 毫米 | 0.5 毫米至 8 毫米 |
最后加工
退火腌制/光亮退火。
管子类型:
U 形弯管和直管
我们进行的部分质量检测包括
腐蚀测试 | 仅在客户特别要求时进行 |
化学分析 | 按照规定的质量标准进行测试 |
破坏性/机械测试 | 拉伸 | 硬度 | 压平 | 扩口 | 法兰 |
反向弯曲和反向平面测试 | 完全符合相关标准和 ASTM A-450 和 A-530 规范,可确保无故障膨胀、焊接和客户端使用 |
涡流测试 | 利用数字瑕疵标记检测系统检测地下的均匀性 |
水压试验 | 100% 静水压力测试根据 ASTM-A 450 标准进行,用于检查管子的泄漏情况,我们可支持的最大压力为 20Mpa/7s。 |
空气压力测试 | 检查是否有漏气迹象 |
目视检查 | 经过钝化处理后,每根管材都要由经过培训的员工进行彻底的目视检查,以发现表面缺陷和其他瑕疵。 |
补充测试 : 除上述测试外,我们还对生产的产品进行补充测试。其中包括
|
|
|