鳍片材料 | Alu.1100 / Alu.1060 | 底管材料 | TP304 / TP304L / TP316L |
---|---|---|---|
管道直径: | 8-51mm | Fin Pitch: | 1.6-10mm |
鳍片高度: | <17mm | Fin THK.: | 0.2-0.4mm |
强光 | Aluminum Composite Fin Tubing, TP304 Steel Composite Fin Tubing, A269 Extruded Finned Tube |
EXTRUDED FINNED TUBE A269 TP304 STEEL ALUMINUM COMPOSITE FIN TUBING
导言
The processing technology of cold-rolled aluminum steel finned tube isthat aluminum tube and steel pipe are first processed into bimetalcomposite pipe,and then the fin is formed after mechanical cold rolling.Based on the physical characteristics of aluminum tube,the finned tubewith steel tube as the core and aluminum fin formed by cold rolling aremade into one.The efficiency of using finned tubes is very high, because the heat dissipation of finned tubes is dozens of times higher than that of ordinary bare tubes due to the winding of fins on the base tube. Moreover, the interior of finned tubes is smooth, and the resistance of the medium flowing in the tubes is small. At this point, not only does it improve the heat transfer efficiency of the finned tube, but it also greatly reduces production costs.
It is widely used in steel, petroleum, chemical industry,machinery, shipbuilding, power station, hospital and food industry.
In fact, using extruded finned tubes is very meticulous, as this type of finned tube can effectively greatly increase the contact area. This further enhances the efficiency of thermal energy conversion and enables more efficient use of energy, achieving better results. Therefore, this is a very environmentally friendly and energy-saving device that can play an effective environmental role.
Extruded finned tube characteristics:
- High heat transfer performance and low contact thermal resistance;
- The contact area between the fin and the tube is large,and the joint istight and reliable;
- Good corrosion resistance and stable long-term service performance;
- The fin has good rigidity and is not easy to deform.
Extruded finned tube applications:
- 钢铁
- 石油
- 化工业
- 机械
- shipbuilding
- power station
- hospital
- food industry
A269 TP304 Equivalent Grades
等级 | UNS 编号 | 老英国 | Euronorm | 瑞典 SS | 日本 JIS | ||
BS | En | 没有 | 名称 | ||||
TP304 | S30400 | 304S31 | 58E | 1.4301 | X5CrNi18-10 | 2332 | SUS 304 |
A269 TP304 化学成分
年级 | 碳 | 铬 | 磷 | 硫磺 | 锰 | 硅 | 镍 |
TP304 | 0.08 | 18.0-20.0 | 0.045 | 0.03 | 2 | 1 | 8.0-11.0 |
A269 TP304 Mechanical Properties
材料 | 温度 | 热量 | 屈服强度 | 拉伸强度 | 伸长率 |
最低华氏度(摄氏度) | 治疗 | Ksi (MPa) | Ksi (MPa) | ||
TP304 | 1900 (1040) | 解决方案 | 30(205) | 75(515) | 35 |
A269 TP304 Physical Properties
等级 | 密度(千克/立方米) | 电阻率 | 弹性模量 | 导热系数(瓦/米.K) | 平均热膨胀系数 (m/m/0C) | 比热 0-1000C (J/kg.K) | |||
---|---|---|---|---|---|---|---|---|---|
在 1000C 时 | 在 5000C 时 | 0-1000C | 0-3150C | 0-5380C | |||||
304/H | 8000 | 720 | 193 | 16.2 | 21.5 | 17.2 | 17.8 | 18.4 | 500 |