AISI 1015 Steel, normalized at 925°C (1700°F), 25 mm (1 in.) round
AISI 1015 Steel, normalized at 925°C (1700°F), 25 mm (1 in.) round Categories: Metal
AISI 1015 Steel, normalized at 925°C (1700°F), 25 mm (1 in.) round Categories: Metal
AISI 1015 Steel, normalized at 925°C (1700°F), 50 mm (2 in.) round Categories: Metal
AISI 1015 Steel, normalized at 925°C (1700°F), 100 mm (4 in.) round Categories: Metal
AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 13 mm (0.5 in.) round Categories: Metal
AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 25 mm (1 in.) round Categories: Metal
AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 50 mm (2 in.) round Categories: Metal
AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 100 mm (4 in.) round Categories: Metal
AISI 1005 Steel Categories: MetalAISI 1005 Low Carbon Steel
AISI 1006 Steel, cold drawn Categories: MetalThe composition listed is for standard grade for wire and rod.