Standard: | ASME / ANSI B16.11, MSS-SP-97, MSS-SP-79, JIS B2316, BS 3799 Etc | Name: | WELDOLET/OLETS FITTING |
---|---|---|---|
Material: | Nickel Alloy HASTELLOY-C22 | Technics: | Forged |
Size: | 1/2′ ~ 60′ | Pressure: | 2000#,3000#,6000#,9000# |
High Light: | C22 Hastelloy Insert Weldolet, Forged Insert Weldolet, Nickel Alloy Pipe Olet Fittings |
ASTM B366 HASTELLOY C22 INSERT WELDOLET NICKEL ALLOY FORGED OLETS FITTING B16.11
What is Weldolet?
Weldolet is the most common among all pipe olet. It is ideal for high pressure
weight application, and is welded onto the outlet of the run pipe. The end are
bevelled to facilitate this process, and therefore the weldolet is consider a
butt weld fitting.Weldolet is a branch butt weld connection fitting that is
adhered to outlet pipe to minimizes stress concentrations. And it provides overall
reinforcement.Normally it has the same or a higher schedule than the run pipe
schedule, and offers a variety of forged material grades, such as ASTM A105, A350, A182 etc.
Hastelloy C22 Weldolet Equivalent Grades
STANDARD | WERKSTOFF NR. | UNS | JIS | EN |
Hastelloy C22 | 2.4602 | N06022 | NW 6022 | NiCr21Mo14W |
Hastelloy C22 Weldolet Specification
Specifications | ASTM B366 / ASME SB366 |
---|---|
Olets Size | 1/8"-4" (DN6-DN100) |
Olets Dimensions | ASME / ANSI B16.11, MSS-SP-97, MSS-SP-79, JIS B2316, BS 3799 etc |
Olets Connect Type | Welded, threaded, BW, SW |
Specialized manufacturer of | Weldolets, Threadolets, Sockolets, Elbolets, Elbolets, Nippolets, Lateral Outlet, Coupolet, Flexolet, Sweepolet, Brazolet |
Test Certificates | EN 10204/3.1B Raw Materials Certificate 100% Radiography Test Report Third Party Inspection Report, etc |
Olets uses & application |
|
Material Test Certificates (MTC) for ASTM B366 Hastelloy C22 Olets as per EN 10204 3.1 and EN 10204 3.2, Test Certificates certifying NACE MR0103, NACE MR0175 |
Chemical Composition
Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
Hastelloy C22 | 0.010 max | 0.50 max | 0.08 max | 0.02 max | 2.50 max | 50.015 min* | 20.00 – 22.50 | 2.00 – 6.00 | 12.50 – 14.50 | 0.02 max |
Mechanical Properties
Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
Hastelloy C22 | 8.69 g/cm3 | 1399 °C (2550 °F) | Psi – 1,00,000 , MPa – 690 | Psi – 45000 , MPa – 310 | 45 % |