ASME SA268 ASTM A268 TP430 Stainless Steel Seamless Tube For Power Plant

Product Details
Place of Origin: CHINA
Brand Name: TONG CHUANG SPECIAL STEEL
Certification: ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008.
Model Number: ASTM A268 TP430 Ferritic Stainless Steels
Payment & Shipping Terms
Minimum Order Quantity: 100KGS
Price: NEGOTIABLE
Packaging Details: Ply-wooden Case /Iron Case/ Bundle with plastic Cap
Delivery Time: 20-80
Payment Terms: L/C, T/T
Supply Ability: 800Tons/ month

SKU: 236 Category:
Specification:ASTM A268 TP430 Ferritic Stainless SteelsTechnique:Cold Drawn
Shape:RoundLength:6 Meters Or Customized
Finish:PickledHeat Treatment:Annealed,pickled Surface
Certification:ISO,SGS,BV,ISO & SGS,ISO/CE/SGSApplication:Power Plant,Hydraulic,energy And Environmental Protection
High Light:

Power Plant Stainless Steel Tube

Ferritic Stainless Steel Tube

A268 TP430 Stainless Steel Tube

ASME SA268 ASTM A268 TP430 Stainless Steel Seamless Tube For Power Plant

We are one of the largest manufacturers of stainless steel, duplex and alloy steel pipes in China. After more than 20 years of development, we have accumulated a large number of customers all over the world, and TONG CHUANG products have won the praise of our customers.
 
ASTM A268 is a standard specification for seamless and welded tubes and pipes of ferritic and martensitic stainless steels for general purposes, in grades TP410, TP405, TP420, TP430, TP430Ti, TP403, TP409, TP444, TP439, and TP446, and ASME SA268 is an alternative standard covering a range of nominal thickness grades of ferritic and martensitic stainless steels. grades of ferritic and martensitic stainless steel welded steel tubing for general corrosion resistance and high temperature environments.
 
Tubing must be seamless or welded with no filler metals added; tubing must be reheated to 1200.F [650.C] or higher and then cooled to meet the requirements of this specification; and all tubing must be free of excessive scale and suitable for inspection. A small amount of oxidation will not be considered scale.

Chemical Composition

Grade:TP410TP430TP439
UNSS41000S43000S43035
C, Max0.150.120.07
Mn,Max111
P, Max0.040.040.04
S, Max0.030.030.03
Si, Max111
Ni0.50max
Cr11.5-13.516.0-18.017.00-19.00
Mo
Al0.15
Cu
N0.04
Ti0.20+4(C+N)Min, 1.10max

Mechanical Properties

GradeTensile Strength, Min, Ksi [MPa]Yield Strength, Min, Ksi [MPa]ELONGATION. MIN, %
TP41055 [380]30 [205]20
TP43060 [415]35 [240]20
TP43960 [415]30 [205]20

Physical Properties

Density, g/cm3 (lb/in.3)7.8 (0.28)
Melting point, °C (°F)1425-1510 (2600-2750)
Specific heat capacity, J/kg · K (Btu/lb · °F)460 (0.11) at 0-100 °C (32 to 212 °F)
Electrical resistivity, μΩ·m0.60 at 20
430 stainless steel magnetic permeability600-1100 (Approximate)
Elastic modulus (Modulus of elasticity), GPa (106 psi)200 (29.0)
Thermal diffusivity, mm2/s7.3
Thermal conductivity, W/m · K (Btu/ft · h · °F)26.1 (15.1), at 100 (212 °F)
26.3 (15.2), at 500 (932 °F)
Coefficient of thermal expansion, μm/m · °C (μin./in. · °F)10.4 (5.8), at 0-100 (32-212 °F)
11.0 (6.1), at 0-315 (32-600 °F)
11.4 (6.3), at 0-538 (32-1000 °F)

SS430 Stainless Steel Heat Treatment

  • Annealing: Recommended annealing treatment for 430 steel is 705-790 °C (1300-1450 °F).
  • Forging: Typical forging temperature for SS430 is 815-1120 °C (1500-2050 °F).

Heat Resistance

Maximum service temperatures, °C (°F)
AISIIntermittent serviceContinuous service
430870 (1600)815 (1500)