Standard: | ASTM A213 / ASME SA213 | Material Grade: | T12 |
---|---|---|---|
Product Name: | Alloy Steel Fin Tube | Type: | High Frequency Welded |
Tube Length: | 18 Meters Max | Application: | Heater Parts,Refrigeration Parts,heat Exchanger,Cooler |
High Light: | Stainless Steel Seamless Fin Tube, Seamless HFW Fin Tube, T12 Heat Exchanger Tube |
ASME SA213 T12 Stainless Steel Seamless HFW Fin Tube Heat Exchanger
T12 steel is used for small wall thickness boilers, superheaters, and heat exchanger tubes. Suitable for seamless iron element and austenitic steel pipes with small wall thickness used in boilers and superheaters, as well as austenitic steel pipes used in heat exchangers.
T12 steel chemical composition: C0.05-0.15 Si ≤ 0.50 Mn 0.30-0.61 P, S ≤ 0.025 Cr0.80.00-1.25 Mo0.44-0.65
Mechanical properties of T12 steel: tensile strength ≥ 415mpa, yield strength ≥ 205mpa, elongation ≥ 30%
The American standard ASTM A213 mainly produces steel pipe grades such as A213T11, A213T12, A213T22, etc.
T12 steel is a grade of steel produced according to the American standard ASTM A213, which does not mean it is produced in the United States. It can be produced by a steel factory in our country according to the American standard ASTM A213, and the quality also meets the American standard.
Working principle of high frequency welded finned tube
The high frequency welding finned tube is welded by the current with a high frequency of 20wHz/s, and the corresponding skin effect and proximity effect will be produced because of the high frequency current welding. The high frequency current of the fin pipe is used as the welding heat source, and the steel strip and steel pipe are heated at the same time to make them integrate.
High frequency welded finned tube is mainly made of steel pipe, steel pipe whether in terms of pressure capacity or heat transfer, is a suitable choice, high frequency welded finned tube in high smoke and high temperature conditions, the radiator is required to have high performance indicators.
High frequency welded fin tube is a kind of radiator that can be used in steam system and hot water system, mainly used in hot air heating, air conditioning system and drying device, and is the main equipment in hot air device.
Chemical Composition:
C, % | Mn, % | P, % | S, % | Si, % | Cr, % | Mo, % |
0.15 max | 0.3-0.6 | 0.025 max | 0.025 max | 0.5-1 | 1-1.5 | 0.44-0.65 |
Mechanical Properties:
Tensile Strength, min, ksi [MPa] | Yield Strength, min, ksi [MPa] | Elongation in 2 in. or 50 mm, min, % | Hardness | |
Brinell | Rockwell | |||
60 [415] | 32 [220] | 30 | 163 HBW | 85 HRB |
Grade | UNS Designation | Composition, % | ||||||
Carbon | Manganese | Phosphorus, max | Sulfur, max | Silicon | Chromium | Molybdenum | ||
T2 | K11547 | 0.10-0.20 | 0.30-0.61 | 0.025 | 0.025 | 0.10-0.30 | 0.50-0.81 | 0.44-0.65 |
T5 | K41545 | 0.15 | 0.30-0.60 | 0.025 | 0.50 | 0.50 | 4.00-6.00 | 0.45-0.65 |
T9 | K90941 | 0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.25-1.00 | 8.00-10.00 | 0.90-1.10 |
T11 | K11597 | 0.05-0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50-1.00 | 1.00-1.50 | 0.44-0.65 |
T12 | K11562 | 0.05-0.15 | 0.30-0.61 | 0.025 | 0.025 | 0.50 | 0.80-1.25 | 0.44-0.65 |
T17 | K12047 | 0.15-0.25 | 0.30-0.61 | 0.025 | 0.025 | 0.5 | 0.80-1.25 | 0.44-0.65 |
T21 | K31545 | 0.05-0.15 | 0..30-0.60 | 0.025 | 0.025 | 0.5-1.00 | 2.65-3.35 | 0.80-1.06 |
T22 | K21590 | 0.05-0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50 | 1.90-2.60 | 0.05-0.30 |
Applications:
Boiler&Heat Exchanger
Steam Generators
Petrochemical Industries
Marine Industries
Refrigeration Applications
Oil and Gas Plants
Plumbing and Air Conditioning
Condensers and Evaporators